Publisher:Gaoseal time:2026-02-06
|
project |
indicator |
|
|
sagging |
Vertical placement,mm |
≤ 3 |
|
horizontally placed |
non-deforming |
|
|
extrudability,s |
≤ 10 |
|
|
Surface drying time,h |
≤ 3 |
|
|
hardness Shore A |
20-60 |
|
|
tensile bond property Mpa |
Standard conditions |
≥ 0.6 |
|
90℃ |
≥ 0.45 |
|
|
-30℃ |
≥ 0.45 |
|
|
after immersion |
≥ 0.45 |
|
|
Water - After exposure to ultraviolet light |
≥ 0.45 |
|
|
Adhesive failure area% |
≤ 5 |
|
|
Elongation at maximum tensile strength at 23 ℃ % |
≥ 100 |
|
|
thermal aging |
Thermogravimetric % |
≤ 10 |
|
crack |
None |
|
|
Powdering |
None |
|
|
project |
indicator |
|
sagging,mm |
≤ 3 |
|
extrudability,ml/min |
≥ 80 |
|
Surface drying time,h |
≤ 3 |
|
Displacement capability % |
±35 / ±25 / ±20 / ±12.5 / ±7.5 not equal |
|
Elastic recovery rate,% |
≥80 |
|
Fixed tensile adhesion |
None |
|
Fixed tensile adhesion after immersion in water |
None |
|
Adhesive properties after cold drawing and hot pressing |
None |
|
Adhesive properties after exposure to heat, artificial light sources through glass, and water |
None |
|
quality loss rate,% |
≤ 8 |